characteristic
X5CRTI17 adds Ti or Nb to X6CR17 steel to reduce the C content and improve the processing performance and welding performance.
use
Used in hot water tanks, hot water supply systems, sanitary appliances, household durable appliances, bicycle flywheels, etc.
chemical composition:
Grade |
C≤ |
Si≤ |
Mn≤ |
S≤ |
P≤ |
Cr |
Ni≤ |
Ti-Nb |
X5CRTI17 |
0.03 |
0.75 |
1.00 |
0.030 |
0.040 |
16.00 19.00 |
0.60 |
0.10 1.00 |
Mechanical properties
Tensile strength σb (MPa): quenching and tempering, ≥363
Conditional yield strength σ0.2 (MPa): quenching and tempering, ≥177
Elongation δ5 (%): quenching and tempering, ≥22
Hardness: annealing, ≤183HB; ≤88HRB; ≤200HV
Heat treatment specifications
Annealing, rapid cooling or slow cooling at 780 ~ 950 ℃;
Delivery status: delivered in annealed condition.
Shenzhen Zhengjie Metal Material Co., Ltd.
Contact person: Mr. Huang (13480167607)
Sales Hotline: 0755-81718772
Q Q: 2263040115 305084123
Website: www.szzj168.com
Email: 2263040115@qq.com
Address: No. 8, Songzi Park, Minzhi, Longhua New District,Shenzhen