4J43 Dumet wire core alloy features
It has a certain linear thermal expansion coefficient in the range of 20 ~ 400 ℃.
4J43 Dumet wire core alloy application
Mainly used in Dumet silk cores.
chemical composition(%)
Alloy |
C≤ |
S≤ |
P≤ |
Si≤ |
Mn |
Ni |
Fe |
4J43 |
0.10 |
0.02 |
0.02 |
0.30 |
0.75~1.25 |
41.00~43.00 |
margin |
Average linear expansion coefficient
Alloy |
Sample processing |
Average linear expansion coefficient a/10-6·K-1 |
20~400℃ |
||
4J43 |
It is heated to 900 ± 20 ° C in a hydrogen atmosphere, kept for 1 hour, and cooled to 200 ° C or lower at a rate of not more than 5 ° C / min. |
6.3~7.2 |
The above data is for reference only. Please contact us for specific requirements.
Shenzhen Zhengjie Metal Material Co., Ltd.
Contact person: Mr. Huang (13480167607)
Sales Hotline: 0755-81718772
Q Q: 2263040115 305084123
Website: www.szzj168.com
Email: 2263040115@qq.com
Address: No. 8, Songzi Park, Minzhi, Longhua New District,Shenzhen