View:1245 Release Time:2017-04-01

4J38 Free cutting low expansion alloy

4J38 free cutting low expansion alloy features

It has a low linear thermal expansion coefficient in the range of 20 ~ 100 , and is easy to cut.

 

4J38 Free cutting low expansion alloy

Various instruments, instrument parts, and resonators that require stable dimensions.

 

chemical composition(%)

Alloy

C

S

P

Si≤

Mn≤

Se

Ni

Fe

4J38

0.05

0.02

0.02

0.20

0.8

0.10~0.25

35.0~37.0

margin

 

Average linear expansion coefficient

Alloy

Sample heat treatment system

Average linear expansion coefficient     a/10-6·K-1

Inflection point

 /℃

20 ℃~400   ℃

4J38

In a protective atmosphere or vacuum, heat to 850 ℃ ~ 900 ℃, keep it for 1 hour, and cool it to below 400 ℃ at a speed of not more than 300 ℃ / h

7.0~9.0

≥390

 

The above data is for reference only. Please contact us for specific requirements

Contact Us

Shenzhen Zhengjie Metal Material Co., Ltd.
Contact person: Mr. Huang (13480167607)
Sales Hotline: 0755-81718772
Q Q: 2263040115 305084123
Website: www.szzj168.com
Email: 2263040115@qq.com
Address: No. 8, Songzi Park, Minzhi, Longhua New District,Shenzhen

Online Service