Precision alloy

4J32, 4J36, Nb-lnvar low expansion alloy

View:1317 Release Time:2017-04-01

4J32, 4J36, Nb-lnvar low expansion alloy

4J32, 4J36, Nb-lnvar expansion alloy features

It has a low coefficient of linear expansion in the temperature range of -60 ° C to 100 ° C.

 

4J32, 4J36, Nb-lnvar expansion alloy applications

Production of various instrumentation components with stable dimensions.

 

chemical composition(%)

Alloy

Mn

Cu

Ni

Co

Fe

4J32

0.20~0.60

0.40~0.80

31.5~33.0

3.20~4.20

margin

4J36

0.20~0.60

-

35.0~37.0

-

margin

Nb-lnvar

0.60

Nb≤0.50

30.0~35.0

3.0~5.0

margin

 

Average linear expansion coefficient

Alloy

Sample processing

Average linear expansion coefficient    a/10-6·K-1

20~100℃

-40~20℃

-20~20℃

4J32

The semi-finished product sample is heated to 840 ± 10 ° C, held for 1 hour, and quenched with water. After the sample is processed into a finished sample, it is held at 315 ± 10 ° C for 1 hour with the furnace cooling or air cooling.

-

≤1.0

-

4J36

-

≤1.5

-

Nb-lnvar

≤0.5

≤0.60

≤0.5

 

The above data is for reference only. Please contact us for specific requirements

Contact Us

Shenzhen Zhengjie Metal Material Co., Ltd.
Contact person: Mr. Huang (13480167607)
Sales Hotline: 0755-81718772
Q Q: 2263040115 305084123
Website: www.szzj168.com
Email: 2263040115@qq.com
Address: No. 8, Songzi Park, Minzhi, Longhua New District,Shenzhen

Online Service